5 / 7 page Temp. ( ℃) Preheat 180~200 ° C Note: 1.Wave solder and reflow soldering should not be made more than one time. 2.You can just only select one of the soldering conditions as above. 120 sec.Max. 1~5 ° C/sec Above 220 ° C 60 sec.Max. 4. PB-Free Reflow Solder 60 ~ 120 sec 260 °C MaX. 10sec.Max 1~5 ° C/sec 5sec Time 120 150 Preheat 240 Rising +5 ℃/sec Cooling -5 ℃/sec 245 ±5℃ within 5 sec 120 ~ 180 sec 3. LEAD Reflow Solder 120 ~ 150 ℃ Preheat Soldering heat Max. 260 ℃ 1. Hand Solder Basic spec is ≦ 280℃ 3 sec one time only. 2. Wave Solder Recommended Soldering Conditions LIGITEK ELECTRONICS CO.,LTD. Property of Ligitek Only Page 4/6 PART NO. L8UG9253-1/S5 |
Similar Part No. - L8UG9253-1-S5 |
|
Similar Description - L8UG9253-1-S5 |
|
|
Link URL |
Privacy Policy |
ALLDATASHEET.NET |
Does ALLDATASHEET help your business so far? [ DONATE ] |
About Alldatasheet | Advertisement | Contact us | Privacy Policy | Link Exchange | Manufacturer List All Rights Reserved©Alldatasheet.com |
Russian : Alldatasheetru.com | Korean : Alldatasheet.co.kr | Spanish : Alldatasheet.es | French : Alldatasheet.fr | Italian : Alldatasheetit.com Portuguese : Alldatasheetpt.com | Polish : Alldatasheet.pl | Vietnamese : Alldatasheet.vn Indian : Alldatasheet.in | Mexican : Alldatasheet.com.mx | British : Alldatasheet.co.uk | New Zealand : Alldatasheet.co.nz |
Family Site : ic2ic.com |
icmetro.com |